SH-DG-400 Pneumatic Dross Grab

Crane-suspended clamshell for bottom dross removal from hot-dip galvanizing kettles. Kettle width ≥ 1,000 mm, depth 1,400–3,200 mm.

Step 1 of 10
Loading model…

View
Jaw angle / shell0.0°
Lip span0 mm

Drag to orbit · pinch or scroll to zoom · Space play/pause · ← → steps · F full screen. While playing, the kettle and furnace turn see-through so the machine stays in view.

    Rated bite400 kgdross, 150 mm layer
    Bowl volume114 Lbowl capacity
    Jaw opening65° · 634 mmlip span, open
    Self weight≈ 526 kgkettle depth 2.6 m

    01How it works

    Two nesting shells hang on one shaft and close like a clamshell. An air cylinder on the mast drives them through links on the shell end plates, so nothing moving passes through the bowl and dross cannot foul the linkage. The grab hangs from the crane, rests on the kettle flanges while it bites, and lifts the dross out with the free zinc draining back through the perforated bowl.

    02Operating procedure

    1. Plan the session. Remove dross after at least 6 h without dipping (overnight settling), bath at normal working temperature. Do not stir the bath before grabbing.
    2. Pre-start checks. 6 bar at FRL; couplings connected; lever CLOSE closes the jaws; pins move freely; lip wear bars intact; hose sleeves in place; rim rest pinned at the set hole on both sides.
    3. Dry the grab. Hang with the shells 200–300 mm above zinc for 10 min. Repeat after any washing, rain or condensation. A wet grab causes a zinc eruption.
    4. Skim and lower. Skim surface ash at the bite position. Open jaws in air, lower at creep speed until the rim rest lands on both kettle flanges. Slack the hook about 50 mm.
    5. Bite. Hold lever at CLOSE until lips meet (≈ 4 s), hold 3 s more, release to centre.
    6. Lift and drain. Take up slack, lift at creep for the first 500 mm. Stop with the bowl 100–200 mm above zinc for 30 s so free zinc drains back through the perforations.
    7. Dump. Traverse at creep to the pre-heated, dry dross moulds. Lower to 150 mm above the mould, OPEN, cycle the jaws twice to shake out.
    8. Next bite. Step 500–600 mm along the kettle per bite, working from one end. Keep cycling the jaws in air between bites while hot, so zinc does not freeze at the pins.
    9. Park. Close jaws, park on the stand over a drip tray, isolate and vent air, disconnect couplings and cap them, return hoses to the reel.
    Exclusion zone 3 m around the kettle while the grab moves. Operator at the valve stand with face shield, aluminised jacket and gloves. Nobody under the suspended grab. Never let the grab strike kettle walls or floor: kettle damage is the costliest failure in the plant. Do not use the grab to lift anything else.