Pickling acid calculator
How much hydrochloric acid your pickling uses, how much spent acid you have to dispose of or regenerate each month, and what one tank charge holds.
What you enter
- Steel pickled, typical 1500 t/mo
- Pickling tanks, typical 3
- Working volume per tank, typical 22 m³
Under Advanced, 3 more inputs for a closer answer, each set to a typical value until you change it: Iron + scale removed 0.8 % of steel; Iron at which the bath is spent 130 g/L; Bath strength when made up 15 % HCl.
What it works out
- Acid 33 %
- Spent acid
- Iron dissolved
- One tank charge
- Tank volume, all tanks
- Bath life (all tanks)
- Pure HCl consumed
- Regeneration
How it works
Fe + 2HCl → FeCl₂ + H₂; about 85 % of the acid charged is used before the bath is spent. Real use depends on the scale, inhibitor, temperature and drag-out. SHIVAS Reinplast builds pickling lines, fume scrubbers, acid recovery and effluent plants.
The answer is a first sizing from typical values, and every input can be changed. Press Ask our engineer to check this under the results and SHIVAS replies with a checked sizing and a proposal.
The equipment it sizes
The same calculator is on each of these pages.
- Pickling plantsPickling plants for strip, wire and batch work: tanks, fume capture, scrubbing and acid management designed as one.
- Wire & wire rod picklingWire and wire-rod pickling: batch coil pickling, and fumeless lines for continuous strands.
- Pipe, tube & structure picklingLong pickling tanks for pipes, tubes and structures, with hoods and acid management.
- Strip pickling linesStrip pickling lines, push-pull or continuous, with PP-H and FRP tanks and fume extraction.
- Pretreatment tanksDegreasing, pickling, rinse, flux and passivation tanks in PP-H, FRP and mild steel, made in our shops and built on the robust side.
- Fumeless pickling lineFumeless pickling lines: wire cleaned in covered tanks with no acid fume in the shed.
- Acid regeneration & recoveryAcid regeneration and recovery plants that return value from spent pickling liquor.
From our engineers
- Pickling right: acid strength, iron and temperatureMost coating defects start before the steel reaches the zinc. How to run hydrochloric acid pickling so it is fast, clean and cheap.
- What to do with spent pickling acid: regenerate, recover or neutraliseSpent acid is a small stream carrying most of the iron and salt. Regeneration, acid recovery, sale and neutralisation compared, with their effect on the ETP.
- Fumeless pickling for wire: keeping the acid inside the tankContinuous wire lines can pickle without filling the shed with acid fume. How covered, controlled tanks change the economics.
- Counterflow rinsing: cleaner work with a fraction of the waterRinse water is most of the effluent in many pickling plants. The counterflow rinse equation, worked examples for one to three stages, and cutting the drag-out.
Other calculators
- Galvanizing plant calculatorKettle, furnace, zinc, fuel and cost per tonne from your steel and tonnage.
- Electro-galvanizing rectifierCurrent, current density and rectifier size
- Wire drawingPasses, die sequence, block speeds, kW and output
- High-velocity burner kWFiring rate, burners, wall heat flux, fuel
- ETP and ZLD plantNeutraliser, sludge, RO, MEE or MVR, ATFD, steam and power
- Coating thickness checkISO 1461 minimums, g/m², zinc per tonne
- Inline phosphating lineBath length, coating time, phosphate and output
- Fume scrubber + blowerAir flow, tower size, packing, pump, blower kW and HP
- Spent acid neutralisationLime, filter cake and dissolved salt
- Bag filterCloth area, bags, housing, fan kW and HP
- Fan / blower motorAir power, shaft kW, motor kW and HP
- FRP profile weight and deflectionkg per metre, steel comparison, beam check